Alle producten
Contactpersoon :
lei
Telefoonnummer :
13266828705
zoekwoorden [ high density polyethylene granules hdpe ] bij elkaar passen 43 producten.
Talsox® 7200 Formosa Kunststof Hdpe
Dichtheid: | 00,955 g/cm3 |
---|---|
Smelte massa-stroom (MFR) (190°C/2,16 kg) 0,05 g/10 min: | 22 g/10 min |
Vervaardiging: | Taiwan Formosa Plastics |
Talsox® 8010 Formosa Kunststof Hdpe
Dichtheid: | 00,956 g/cm3 |
---|---|
Smelte massa-stroom (MFR) (190°C/2,16 kg) 0,05 g/10 min: | 1 g/10 min |
Vervaardiging: | Taiwan Formosa Plastics |
Purell Gb7260 Lyondellbasell Hdpe
Dichtheid (23°C): | 00,96 g/cm3 |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 8 g/10 min |
Verwerkingsmethode: | Injectievorming |
Braskem SHA7260 Plastic HDPE suikerriet polyethyleengranulaat van plantaardige oorsprong
Dichtheid (23°C): | 00,955 g/cm3 |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 20 g/10 min |
Gecoupleerde Izod Impact (23°C): | 20 J/m |
Talsox® 9003 Formosa Kunststof Hdpe
Dichtheid: | 00,952 g/cm3 |
---|---|
Smelte massa-stroom (MFR) (190°C/2,16 kg) 0,05 g/10 min: | 0.25 g/10 min |
Vervaardiging: | Taiwan Formosa Plastics |
Groen PE-materiaal Braskem SHC7260 Biobased Plastic HDPE Polyethyleengranules
Dichtheid (23°C): | 00,959 g/cm3 |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 7.2 g/10 min |
Gecoupleerde Izod Impact (23°C): | 20 J/m |
Lutene® ME2500 LG Chem HDPE
Density: | 0.958 g/cm³ |
---|---|
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg): | 0.25 g/10 min |
Durometer Hardness (Shore D): | 64 |
Braskem SHD7255LS-L Biobased Plastic HDPE Particles Suikerriet Polyethyleengranulaten
Dichtheid (23°C): | 00,954 g/cm3 |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 4.5 g/10 min |
Gecoupleerde Izod Impact (23°C): | 20 J/m |
Braskem PE HA7260 HDPE-deeltjes voor injectie Polyethyleengranules
Dichtheid (23°C): | 00,955 g/cm3 |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 20 g/10 min |
Gecoupleerde Izod Impact (23°C): | 20 J/m |
Hiden® M850 Yuhwa Korea
Dichtheid: | 0.965 g/cm3 |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 4.7 g/10 min |
Rockwellhardheid (R-schaal): | 56 |