EngageTM 8450 Polyolefin Elastomer Dow Inc.
Dichtheid (G/Cm3): | 0,902 g/cm ³ |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 1.0 g/10 min |
Formulieren: | Pellets |
EngageTM 8180 Polyolefin Elastomer Dow Inc.
Dichtheid (G/Cm3): | 00,863 g/cm3 |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 0.5 g/10 min |
Formulieren: | Pellets |
EngageTM 7447 Polyolefin Elastomer Dow Inc.
Dichtheid (G/Cm3): | 00,865 g/cm3 |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 5 g/10 min |
Kust A: | 64 |
EngageTM 8402 Polyolefin Elastomer Dow Inc.
Dichtheid (G/Cm3): | 00,885 g/cm3 |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 1.0 g/10 min |
Kust A: | 84 |
EngageTM 8100 Polyolefin Elastomer Dow Inc.
Dichtheid (G/Cm3): | 0.87 g/cm3 |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 1.0 g/10 min |
Kust A: | 73 |
EngageTM 8150 Polyolefin Elastomer Dow Inc.
Strand A, 1 seconde, gevormd door compressie: | 70 |
---|---|
Dichtheid (G/Cm3): | 0.868 g/cm3 |
Productnaam: | Thermoplastisch Elastomeer |
EngageTM 8200 Polyolefin Elastomer Dow Inc.
Dichtheid (G/Cm3): | 0.87 g/cm3 |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 5 g/10 min |
Formulieren: | Pellets |
EngageTM 8480 Polyolefin Elastomer Dow Inc.
Dichtheid (G/Cm3): | 0,902 g/cm ³ |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 1 g/10 min |
Kust A: | 89 |
EngageTM 8003 Polyolefin Elastomer Dow Inc.
Dichtheid (G/Cm3): | 00,885 g/cm3 |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 1.0 g/10 min |
Kust A: | 84 |
EngageTM 7467 Polyolefin Elastomer Dow Inc.
Dichtheid (G/Cm3): | 00,862 g/cm3 |
---|---|
Melt mass-flow rate (MFR) (190°C/2,16 kg): | 1.2 g/10 min |
Kust A: | 52 |